The equivalent to buy is a 5502 in the same melt index class as the one in your spec, measured at 190 °C / 2.16 kg. The number “5502” alone does not make two grades interchangeable. Producers sell 5502s at three melt indexes, and each class goes to different containers:
- Lightweight bottles: detergent, household-chemical, pharmaceutical and personal-care bottles run on the 0.35 g/10 min class.
- Large rigid parts, or a spec already at 0.25: totes, coolers and storage sheds, and some household and cosmetics packaging, run on the 0.25 g/10 min class.
- Containers up to 30 liters on a 0.2 spec: the 0.2 g/10 min class is the only one whose sheets state a container-size limit.
Your current spec or certificate of analysis tells you which case is yours. Read the melt index and check that it was measured at 2.16 kg.
Within one class, the MI and density on the data sheets barely differ, so they rarely rule a candidate out. ESCR separates the candidates, but only when the test agent, its concentration and the test method match.
Which 5502 Does Your Spec Describe?
Your spec describes a particular 5502 only when it gives both the melt index at 2.16 kg and the producer. Many producers sell a grade numbered 5502, at melt indexes of 0.2, 0.25 or 0.35 g/10 min, so a spec that says only “HDPE 5502” does not pin down a grade.
| Producer | Grade | MI, 190 °C / 2.16 kg (g/10 min) | Producer’s stated use |
|---|---|---|---|
| CPChem | Marlex HHM 5502LW, 5502LD | 0.35 | Detergent bottles, household and industrial chemical containers |
| CPChem | Marlex HHM 5502BN, 5502BZ | 0.35 | Lightweight and pharmaceutical containers; 5502BZ also injection blow molded containers |
| CPChem | Marlex HHM 5502-01ST | 0.25 | Sheet, thermoforming and blow molded large parts: tote boxes, coolers, storage sheds |
| Baystar | HDPE 5502 | 0.35 | Bleach and detergent containers, industrial chemical containers, food packaging |
| Formosa | Formolene HB5502B, HB5502F, HB5502Z | 0.35 | Household chemical bottles (B); motor oil, olive oil and shampoo bottles (F); toiletry and pharmaceutical bottles, injection blow molding (Z) |
| Q-Chem | Lotrène Q 5502BN | 0.35 | Lightweight containers for household chemicals, food and pharmaceuticals |
| TotalEnergies | HDPE 5502 (produced in Europe) | 0.25 | Household, industrial and cosmetics liquid packaging |
| INEOS | Rigidex HD5502S | 0.2 | Containers up to 30 liters for chemicals, household products, oils and foodstuff |
| SIDPEC | HD5502GA | 0.2 | Containers up to 30 liters |
| OPaL | HDPE B5502 (provisional sheet) | 0.2 | General purpose containers up to 30 liters |
Chinese plants add their own: Shandong Yulong’s HD5502S, a chromium-catalyzed unimodal grade for small hollow containers, and PetroChina’s HD5502XA.
The suffix after “5502” is each producer’s private code, so it cannot be matched across producers. The same string can even name two different resins: INEOS and Shandong Yulong both sell an “HD5502S”. Write the producer into the spec along with the grade.
Food-contact and pharma clearance is also set per grade. The Q-Chem Q 5502BN sheet lists FDA 21 CFR 177.1520 and a Drug Master File listing. The TotalEnergies HDPE 5502 sheet states that its products are not suitable for pharmaceutical or medical applications unless specifically indicated. A pharma bottle spec cannot move between those two grades on the number alone.
The Melt Index, HLMI and Density a 5502 Equivalent Has to Match
A 5502 equivalent has to match the melt index at 190 °C / 2.16 kg, the load at which every 5502 sheet in the table above prints its headline MI. A spec whose headline flow figure is measured at 21.6 kg describes a different kind of resin: a high-molecular-weight grade for 1–25 liter containers and larger parts. Such a grade is no 5502 substitute, whatever its density.
Read the printed MI as a nominal class value. The sheets state typical properties, not specification limits.
Density does little to tell 5502s apart. The 5502 sheets that print density all give 0.954 or 0.955 g/cm³. A candidate well away from 0.955 g/cm³ is a different kind of grade.
HLMI helps only when both sheets print it on the same standard, and most 5502 sheets leave it blank.
Two grades with the same MI can still differ in shear sensitivity and run differently on the head. A less shear-sensitive grade can need a higher melt temperature and a longer cycle, and can give weak parisons that pleat or web in the handle. A 5502 data sheet gives no shear-sensitivity figure, so only a line trial settles it between two grades of equal MI.
Comparing ESCR Across 5502 Data Sheets
ESCR figures from two 5502 sheets compare only when both use the same test, the same agent and the same concentration. Most published 5502 figures use ASTM D1693 Condition B with F50 in hours, but the agent and its strength vary:
| Grade | ESCR, F50 (h) | Agent and concentration | Test | MI, 2.16 kg (g/10 min) |
|---|---|---|---|---|
| Baystar HDPE 5502 | 50 | 100% Igepal | ASTM D1693, Condition B | 0.35 |
| Baystar HDPE 5502 | 35 | 10% Igepal | ASTM D1693, Condition B | 0.35 |
| CPChem Marlex HHM 5502BN | 24 | 100% Igepal | ASTM D1693, Condition B | 0.35 |
| Formosa Formolene HB5502F | 30 | 100% Igepal | ASTM D1693, Condition B | 0.35 |
| Q-Chem Lotrène Q 5502BN | 24 | 100% Igepal | ASTM D1693, Condition B | 0.35 |
| INEOS Rigidex HD5502S | 50 | 100%, 50 °C (agent not named) | ASTM D1693 bent strip | 0.2 |
| TotalEnergies HDPE 5502 | 60 | 100% Antarox | ASTM D1693, Condition B | 0.25 |
| OPaL HDPE B5502 (provisional sheet) | 200 | 10% Igepal | ASTM D1693, Condition B | 0.2 |
| SIDPEC HD5502GA | 25 | Not stated | ASTM D2561 bottle test, 50 °C | 0.2 |
Small gaps between sheets are inside the test’s own scatter. When different laboratories run ASTM D1693, a material that fails at F50 = 10 h in one lab can be expected to score anywhere from 3.4 to 29 h in others. Read 24 h against 30 h as no measured difference. Where the margin matters to your bottle, or where the two sheets use different agents or tests and cannot be lined up at all, ask each supplier for a figure on your basis or test both grades side by side on the same equipment.
Sheets from Chinese plants often cite GB/T 1842 instead of ASTM D1693. GB/T 1842-2008 is a modified adoption of D1693, so ask for the condition, agent and concentration behind a GB/T 1842 figure before placing it next to D1693 rows.
Which 5502 Melt Index Fits Your Containers
Stay in the MI class your line already runs. That means 0.35 g/10 min for lightweight bottles, 0.25 g/10 min for large rigid parts or a 0.25 packaging spec, and 0.2 g/10 min for containers up to 30 liters.
Crossing classes changes how the line runs. A 0.25 grade in place of a 0.35 one needs a melt temperature toward the top of the 175–205 °C HDPE range at the die head. A 0.35 grade in place of a 0.25 one sags more on a long parison.