How to Choose an HDPE Film Grade for Blown Film

Choose a high-molecular-weight (HMW) HDPE grade for thin, strong film such as carrier bags, T-shirt sacks and can liners, and a medium-molecular-weight (MMW) grade for general packaging, lamination film, coextrusion layers and blending into LDPE or LLDPE. Moisture-barrier film is the exception: the HMW grade’s strength comes with poorer barrier, so barrier film takes the highest-density grade with a higher melt index and a narrower molecular weight distribution.

Once the film type has settled the family, check the grade against your line, because an HMW grade will not run on every line. HMW grades are made for a high-stalk bubble and often need a grooved-feed extruder. If you run an LDPE-style line, with the bubble in the pocket and a smooth-bore extruder, look for an HDPE film grade whose data sheet was measured under those conditions. These are usually MMW grades.

HMW or MMW: Match the Grade to the Film

HMW grades suit thin film that has to be strong: carrier bags, merchandise and grocery sacks, freezer film and can liners. MMW grades give up some of that strength for easier processing and are sold for general packaging, lamination film, coextrusion layers and collation shrink film.

MMW grades are also the HDPE you blend into LDPE or LLDPE for stiffness.

For moisture-barrier film, such as liners for cereal and cracker boxes, the HMW grade is the wrong pick. Look for a higher melt index and a narrower molecular weight distribution, which give better barrier.

Read Melt Index at the Load the Grade Is Quoted

Compare HDPE film grades only on melt indices measured at the same load. One resin reads very differently at 2.16, 5 and 21.6 kg, and producers quote HMW and MMW grades at different loads. HMW grades flow so little at 2.16 kg that LyondellBasell puts its HMW film resins at 0.03 to 0.1 g/10 min at 190 °C/2.16 kg.

Grade (producer)Producer’s labelMI at 190 °C/2.16 kg (g/10 min)MI at 190 °C/5 kg (g/10 min)MI at 190 °C/21.6 kg (g/10 min)
HTA001HD5 (ExxonMobil)HMWnot given0.329.0
HTA002HD5 (ExxonMobil)MMWnot given0.6816
HTA108 (ExxonMobil)MMW homopolymer0.70not given46
HF3728 (Formosa)MMW0.30not given20
7000F (MOL)Bimodal0.080.309.0
FS 471-02 (MOL)Unimodal0.180.8015

Check the load before you call a grade high-flow. A melt index of 9.0 g/10 min at 190 °C/21.6 kg puts a grade in the same band as ExxonMobil’s HMW grades, which read 9.0 and 9.5 at that load. A grade quoted that way belongs to the lowest-flowing HDPE film family, even when it is sold as a high-flow grade for fast lines.

Density for HDPE Film Grades

HDPE film grades run from about 0.937 to 0.962 g/cm³, and a step up in density gives better moisture barrier and stiffness at the cost of tear and dart. Pick the highest density for barrier film, and a lower-density grade where tear and dart matter more than barrier.

Unimodal or Bimodal

Pick a bimodal grade when a steadier bubble matters more than moisture barrier and you run an HDPE stalk line. Its broad distribution lets it extrude at a lower melt temperature, which steadies the bubble, but the same broad distribution gives poorer moisture barrier.

The lower-melt-temperature claim comes from producers of bimodal grades: Borealis says it for its Borstar HDPE, and Formosa for its bimodal HMW film resins against other HMW resins. Whether a bimodal grade runs a steadier bubble than your unimodal one is something a trial on your line settles.

Do not treat a unimodal and a bimodal grade as interchangeable because their melt index and density match.

Match the Grade to Your Line’s Bubble and Extruder

HMW grades need a high-stalk bubble and often a grooved-feed extruder; MMW grades run on smooth-bore extruders, and some of them on LDPE-style pocket lines. The quickest check is the test-line note under the data sheet’s film properties, because it describes the line the grade was made for.

Grade (producer)Producer’s labelBlow-up ratioFrost lineDie gap (mm)
HTA001HD5, HTA002HD5 (ExxonMobil)HMW, MMW4:19 × die diameter1.0
HF3728 (Formosa)MMW4:17 × die diameter (56 in on an 8 in die)0.89 (0.035 in)
FB1460 (Borouge)Bimodal HDPE4:18 × die diameter1.2
HTA108 (ExxonMobil)MMW homopolymer2.5:1Pocket extrusionnot given
Alathon L5885 (LyondellBasell)MMW homopolymer2.5:1not given1.5 (60 mil)

The first three grades were tested on stalk lines, at a 4:1 blow-up ratio and a frost line 7 to 9 times the die diameter. The last two were tested at 2.5:1, and HTA108’s note names pocket extrusion.

Producers disagree on the extruder. Formosa says its HMW grades cannot be processed effectively on a smooth-bore extruder; its MMW grades run on either. LyondellBasell says customers run its bimodal HMW grade Alathon L4907 on both grooved-feed and smooth-bore equipment. If your extruder is smooth-bore, take an HMW grade only when its producer says it runs on one.

A line designed for LDPE narrows the choice further, toward the low-density end of the HDPE film range and below it. MOL, for example, clears four of its grades for machines designed for LDPE. Three of them sit at 0.935 to 0.938 g/cm³, and the fourth, FB 472-02, is 0.947 g/cm³. On such a line, take only a grade whose producer clears it for LDPE equipment or whose test-line note shows pocket conditions.

Newsletter Updates

Enter your email address below and subscribe to our newsletter